Investigation of Microstructure, Adhesion Strength and Wear Resistance of Coatings Being Obtained with Combined Method
This paper deals with a state-of-the-art two staged coating technology involving Cold Gas Dynamic Spraying (CGDS) followed by treatment of the sprayed layer by Micro Arc Oxidation (MAO). This technology provides good ...